Overview

Bulk density g/cm3: ≥4.00

Apparent Porosity %: ≤1.2

Cold Crushing Strength Mpa: ≥300

Exudation Temperature of Glass Phase: ≥1410

Bubble Separation Ratio(1300℃×10h): ≤1.0

Anti-corrosion rate of glass liquid 1500℃×36h (mm/24h)%:

Feature

TY- AZS41 Shapes and sizes:

this product is available in a large size straight or approximate bricks and special formats and shapes which are available for special machining processes.

TY- AZS41 Application:

Mainly used for sidewalls, doghouses, throat, bottom budding, Dam blocks, electric block corners.

Advantages:

Compact microstructure Good erosion resistibility to molten glass Good thermal shock resistibility Barely rendering blister

Technical Data
Item Behaviors
  TY-AZS41
Chemical Composition Al2O3 ≥45.00
  ZrO2 ≥40.50
  SiO2 ≤13.00
  Na2O+K2O ≤1.30
Bulk density g/cm3 ≥4.00
Apparent Porosity % ≤1.2
Cold Crushing Strength Mpa ≥300
Exudation Temperature of Glass Phase ≥1410
Bubble Separation Ratio(1300℃×10h) ≤1.0
Anti-corrosion rate of glass liquid 1500℃×36h (mm/24h)% ≤1.2
Apparent density (g/cm3) PT(RN RC N) ≥3.70
  ZWS(RR EVF EC ENC) ≥3.90
  WS( RT VF EPIC FVP DCL) ≥4.00

Need more information? Drop us a line

For more information on any of our products please get in touch using the form below. One of our sales team will respond to your enquiry as soon as possible.

Copyright © 2014 Zhengzhou Sunrise Refractory Co., Ltd. Site Index Product IndexSitemap   

main products:Fused Cast Alumina Block,  Fused Cast High Zirconia Block,  Fused Cast Skid Rail Block