Item: Silica Insulation Brick
SiO2: ≥88%
Bulk Density: ≤0.85 g/cm3
0.2Mpa Refractoriness Under Load T0.6: ≥1.0℃
Permanent Linear Change On Reheating(%)1450℃X2h: 0~+0.5
Thermal Conductivity (W/MK) 350℃: 0.55
It is mainly made of top class silica, via shaping and burning under the high temperature, possesses high temperature resistant, high strength and low impurities, etc.
▶ Advantage:
◆ Good thermal insulaton effects;
◆ Good acid erosion resistance;
◆ High softening point with temperature;
◆ No shrink in burn repeatedly.
Stable Capability, High Quality, Excellent Service, Competitive price is the most important advantage of our products.
▶ Application:
The main applications are the low temperature parts such as blast furnaces and hot blast furnaces, waste incinerators and glass melting furnaces.
Item | QG-0.8 | QG-1.0 | QG-1.1 | QG-1.15 | QG-1.2 |
SiO2 (%) | ≥88 | ≥91 | ≥91 | ≥91 | ≥91 |
Bulk Density (g/cm3) | ≤0.85 | ≤1.00 | ≤1.10 | ≤1.15 | ≤1.20 |
Cold Crushing Strength (Mpa) | ≥1.0 | ≥2.0 | ≥3.0 | ≥5.0 | ≥5.0 |
0.2Mpa Refractoriness Under Load T0.6 (℃) | ≥1400 | ≥1420 | ≥1460 | ≥1500 | ≥1520 |
Permanent Linear Change On Reheating (%) 1450℃X2h | 0~+0.5 | 0~+0.5 | 0~+0.5 | 0~+0.5 | 0~+0.5 |
20-1000℃ Thermal Expansich10-6 (℃) | 1.3 | 1.3 | 1.3 | 1.3 | 1.3 |
Thermal Conductivity (W/MK) 350℃ | 0.55 | 0.55 | 0.60 | 0.65 | 0.70 |
For more information on any of our products please get in touch using the form below. One of our sales team will respond to your enquiry as soon as possible.